Figure 4: Fully tempered glass after heat-soak testing. Some of the glass remains unbroken (i.e. has passed the test), whereas some has fractured as result of the NiS-inclusion phase transformation during heating in the furnace. Photo courtesy Agnora.

Figure 4: Fully tempered glass after heat-soak testing. Some of the glass remains unbroken (i.e. has passed the test), whereas some has fractured as result of the NiS-inclusion phase transformation during heating in the furnace.
Photo courtesy Agnora.