Figure-5_Image-courtesy-of-Simpson-Gumpertz-&-Heger

View of “cat-eye” fragments at fracture origin (arrows), typical of nickel sulfide- (NiS) induced fracture of fully tempered glass, with no apparent crushing of the glass surface. Photo courtesy Simpson Gumpertz & Heger

View of “cat-eye” fragments at fracture origin (arrows), typical of nickel sulfide- (NiS) induced fracture of fully tempered glass, with no apparent crushing of the glass surface.
Photo courtesy Simpson Gumpertz & Heger