Figure 7

Figure 7: Mineral fiber acoustical panels were disfigured by almost all other staining agents tested, including this specimen tested with red wine. Thermoformed acoustic panels were resistant to all but a few of the agents tested. Photos © National Testing Systems

Figure 7: Mineral fiber acoustical panels were disfigured by almost all other staining agents tested, including this specimen tested with red wine. Thermoformed acoustic panels were resistant to all but a few of the agents tested.

Photos © National Testing Systems